Stainless Melt Extracted Steel Fibers for Furnace Lid Materials

Product Details
Customization: Available
Material: Stainless Steel
Refractoriness (℃): 1580< Refractoriness< 1770
Still deciding? Get samples of US$ 0/KG
Order Sample
Shipping & Policy
Shipping Cost: Contact the supplier about freight and estimated delivery time.
Payment Methods:
visa mastercard discover JCB diners club american express T/T
PIX SPEI OXXO PSE OZOW
  Support payments in USD
Secure payments: Every payment you make on Made-in-China.com is protected by the platform.
Refund policy: Claim a refund if your order doesn't ship, is missing, or arrives with product issues.
Secured Trading Service
Gold Member Since 2016

Suppliers with verified business licenses

Audited Supplier

Audited by an independent third-party inspection agency

Find Similar Products

Basic Info.

Model NO.
ML310/25/. 60ST
Standard
ASTM A820
Aspect Ratio
42
Feature
Long Time Materials
Type
Refractory Material
Transport Package
50*20kg Cartons Then on Fumigation Pallet
Specification
0.6mm*25mm
Trademark
HARVEST
Origin
Dalian, China
HS Code
73269090
Production Capacity
500mt/Month

Product Description

Melt Extracted Stainless Steel Fiber

Chemical composition

Steel Grade C Si S P Mn Ni Cr Mo V Cu Ti Co B
446 <0.30 <3.0 <0.03 <0.04 1.0~1.5 0.45 24-27 - - <0.25 - -

<0.003

The Specification Of Melt-extraction SSF

Specification Cross-section areas(mm2) Equivalent diameter(mm) Cross-section size(mm) Length(mm) Configuration & shape
 0.5*20    0.2    0.5    0.2*1  20   Straight
 0.5*25  25
 0.5*35  35

Technical Properties And Performance

Alloy 446
Melt temperature range ºC 1430~1510
Thermal conductivity @ 540ºC Kcal/m2 · h · ºC 69.8
Modulus of elasticity @ 870ºC × 106kg/cm ² 0.984
Fiber tensile strength @ 870ºC kg/cm ² 540
Coef. of thermal expansion @870ºC × 10-6/ºC 13.14
Critical oxidation temperature ºC 1200

Increased flexural strength of 60% alumina

Refractory fired at 870ºC(1600ºF)for 8hrs 1.3.V% fiber

  1.15
Increased energy absorption 60% alumina ref. fired at 870ºC(1600ºF) for 8 hrs   10-12
Carburization increase in carbon content% in 25 hrs @982ºC(1800ºF)   0.07
Corrosion rate in Coke oven gas at 982ºC(1800ºF) Mils/yr 14
Corrosion rate nitriding Mils/yr 1120
Oxidation cycling coditions 1000 hrs wt % loss @ 982ºC(1800ºF)   4%



Stainless Melt Extracted Steel Fibers for Furnace Lid Materials
The properties and performance of refractory materials applying to various beating furnaces kilns and coke ovens should be greatly improved if SSF will be mixed with.

Today SSF reinforcement is finding its way into every parts of modern industries. They can be concluded as follow:

1)Metallurgical industry

blast-heating cupola, iron smelting furnaces, open hearth furnaces, convertors electrical furnaces, spray gun for refining of metal out of furnace, sintering furnaces and kilns. heaters for steel rolling, including lining, furnace-door and wrapping covers around water cycling pipes.

2)Oil oven, and kilns.

3)Furnaces and kilns in ceramic,glass and enamel industries.

4)Rotary and standing kilns in cement industry.

5)Forging heaters and boilers for power plant.

6)Furnaces and kilns in other industries.

Stainless Melt Extracted Steel Fibers for Furnace Lid Materials


Stainless Melt Extracted Steel Fibers for Furnace Lid Materials

Welcome to contact us !
Stainless Melt Extracted Steel Fibers for Furnace Lid Materials

Send your message to this supplier

*From:
*To:
*Message:

Enter between 20 to 4,000 characters.

This is not what you are looking for? Post a Sourcing Request Now
Contact Supplier